Neste-raskas polttoöljy LS 420
Produktnummer 170380
Paketstorlekar
- Bulk / kg
Typiska egenskaperTypiska egenskaper
1.1.2025
Ash
Min: -
Max: 0.1
wt-%
ISO 6245
Asphaltenes
Reported
mg/kg
DIN 51595
Burning catalyst
Added²⁾
Carbon
Reported
wt-%
ASTM D5291
Carbon residue micromethod
Min: -
Max: 18
wt-%
ISO 10370
Density 15 °C
Min: 920
Max: 1020
kg/m³
EN ISO 12185
Flash point
Min: 60
Max: -
°C
ISO 2719
Kinematic viscosity @ 50 °C
Min: 220
Max: 415
mm²/s
ISO 3104
Kinematic viscosity @ 80 °C
Min: 48
Max: 78
mm²/s
ISO 3104
Net heat of combustion
Min: 40.1
Max: -
MJ/kg
ASTM D240
Nickel
Reported
mg/kg
IP 501
ISO 10478M
NM122
ISO 10478M
NM122
Nitrogen
Reported
wt-%
ASTM D5291
Pour point
Min: -
Max: 30
°C
ASTM D 5950
ISO 3016
ISO 3016
Sulfur
Min: -
Max: 1.00
wt-%
EN ISO 8754
NM380
NM380
Total sediment
Min: -
Max: 0.15
wt-%
ISO 10307-1
Vanadium
Reported
mg/kg
IP 501
ISO 10478M
NM122
ISO 10478M
NM122
Water
Min: -
Max: 0.7
wt-%
ISO 10336
ISO 3733
ASTM D 6304 C
ISO 3733
ASTM D 6304 C

Neste-raskas polttoöljy LS 420
Typiska egenskaper
Ash | Min: - | Max: 0.1 | wt-% | ISO 6245 |
Asphaltenes | Reported | mg/kg | DIN 51595 | |
Burning catalyst | Added²⁾ | |||
Carbon | Reported | wt-% | ASTM D5291 | |
Carbon residue micromethod | Min: - | Max: 18 | wt-% | ISO 10370 |
Density 15 °C | Min: 920 | Max: 1020 | kg/m³ | EN ISO 12185 |
Flash point | Min: 60 | Max: - | °C | ISO 2719 |
Kinematic viscosity @ 50 °C | Min: 220 | Max: 415 | mm²/s | ISO 3104 |
Kinematic viscosity @ 80 °C | Min: 48 | Max: 78 | mm²/s | ISO 3104 |
Net heat of combustion | Min: 40.1 | Max: - | MJ/kg | ASTM D240 |
Nickel | Reported | mg/kg | IP 501 ISO 10478M NM122 | |
Nitrogen | Reported | wt-% | ASTM D5291 | |
Pour point | Min: - | Max: 30 | °C | ASTM D 5950 ISO 3016 |
Sulfur | Min: - | Max: 1.00 | wt-% | EN ISO 8754 NM380 |
Total sediment | Min: - | Max: 0.15 | wt-% | ISO 10307-1 |
Vanadium | Reported | mg/kg | IP 501 ISO 10478M NM122 | |
Water | Min: - | Max: 0.7 | wt-% | ISO 10336 ISO 3733 ASTM D 6304 C |